Instructions for the nano coating process

纳米涂层制作流程介绍

 

    If nano layers on your coated plates are destroyed, you can coat them again. Here are the Instructions.

    如果你的金属板上的纳米涂层被破坏了,你可以重新给它们制作涂层。下面是流程介绍。

 

1. Prepare plastic container with cover

1. 准备好一个有盖子的塑料容器。

 

2. Put a wire mash at the bottom of the container, so that material which will be coated doesn't touch the bottom of the container.

2. 在塑料容器的底部放置一块金属网,目的是防止准备制作涂层的材料和塑料容器的底部发生接触。

 

3. Put about 30 to 40 g of Sodium Hydroxide (NaOH) evenly at the bottom o the container - depending on the size of the container and on what kind of material you are coating. If you want to coat brass, you need to use more NaOH than if you want to coat copper, for example.

3. 将大约30~40克氢氧化钠(NaOH)均匀撒到塑料容器的底部——这取决于容器的大小以及你打算在什么材料上面做涂层。例如,如果你想要给黄铜做涂层,你需要使用比做铜的涂层时更多氢氧化钠。

 

4. Put the metals that you want to coat onto the mesh in the container

4. 将准备制作涂层的金属材料放置在容器中的铁丝网上。

 

5. Boil water, then pour that boiling water into the container with NaOH and metals inside, so that the metals are covered with water. You have to be extremely careful furing this step, because boiling water reacts with NaOH and ca spout at your body.

5. 烧开水,然后开水倒入放有氢氧化钠以及金属的容器内,让水面盖过金属材料。这个步骤你必须格外地小心,因为开水与氢氧化钠反应可能会喷涌到你身体上。

 

6. Leave the matals in the NaOH solution for two days.

6. 让金属材料在氢氧化钠溶液中浸泡两天。

 

7. After two days, put the nano coated plates into another container with a metal mesh at the bottom. Add some of the liquid from the first container - just to cover tha bottom of the new container - this will bive you moist environment.

7. 两天之后,将制作了纳米涂层的金属板放置到另一个底部放置有铁丝网的容器。加入第一个容器中的一些液体,只需要覆盖新容器的底部就可以——这会制造一个潮湿的环境。

 

8. Measure the voltage across the nano coated metal in such a way that you put one electrode of the volt-meter on the metal mash at the bottom, and with the other electrode you touch once each metal piece at one spot for few seconds. The volt-meter should be set to a range of 200 mV or 2 V. This should be done quickly so that the metals don't start drying. Close the cover of the container after measuring and let the nano layers grow for a day or two.

8. 测量横穿做了纳米涂层的金属板的电压,测量方式如下:电压表的一个电极放在地下的金属网上,然后用另一个电极触碰每一块金属材料的一个点几秒钟。电压表应该设定在200mV或2V档。这个过程要快速完成,为了不让金属材料开始变干燥。完成测量后盖好容器,让纳米涂层生长一天或两天。

 

9. Dry nano coated plates or other metals very slowly - you slightly open the cover of the container where you are growing your nano material. It depens on the moisture of the air- this takes a day or two.

9. 慢慢地干燥做了纳米涂层的金属板或其他金属材料——稍微打开那个正在生长纳米材料的容器的盖子。这个步骤取决于空气湿度——可能需要一天或两天。

 

10. This step is only optional. When you finish the first coating, you can do another steaming process. this means that you hand material that you are coating from the top of the container. When you pour water onto the NaOH, the materials you are coating should not be submerged in the water, but only steamed in hot vapor, which creates enough energy so that atoms are pulled from the molecular structure and create a nano layer at the top. 

10. 这个步骤只是选择性的。当你完成了第一次涂层制作后,你可以做另一个熏蒸的过程。就是说,将你要制作涂层的材料挂在容器的顶部。你将开水倒到氢氧化钠上时,不要将你要制作涂层的材料浸入水中,只是让它们在热腾的蒸汽中熏蒸,这样的熏蒸会产生足够的能量,从而将原子从分子结构中拉出来并在材料表面形成纳米涂层。

 

11. After steaming repeat step 8.

11. 熏蒸完成后重复步骤8。

 

12. Before you use nano coated plates or other metals, you should wash them in the water, by submerging them in the water for a moment. This way you clean the caustic from the nano layers. Then you leave them in the open air to dry.

12. 在使用已经制作了纳米涂层的金属板或其他金属之前,你应该在水里清洗它们,就是将它们浸泡在水里一段时间。如此就能清除纳米涂层上的碱然后将它们放置在空气中晾干。

 